Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.40e+11 ohm-cm @Temperature 65.6 °C |
2.40e+11 ohm-cm @Temperature 150 °F |
|
Abatron AboCast 8-9/Abocure 8-9 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 480 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh.. |
|||
Electrical Resistivity | 2.40e+11 ohm-cm @Temperature 93.3 °C |
2.40e+11 ohm-cm @Temperature 200 °F |
|
Abatron AboCast 8-15/Abocure 8-15 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/11.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 70 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |