Polymer Property : Flexural Strength = 76.88 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 76.88 MPa
11150 psi
Abatron AboCast 8-9/Abocure 8-9 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 480 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh..