ATI Allvac® Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer ATI Allvac
Trade Name Vasco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Compressor blades, vanes, disks, shafts, wheels, fasteners, gas turbine and jet engine components.
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 130
130
As reported by the manufacturer. Beyond normal Rockwell B hardness range.
Tensile Strength, Ultimate 1172 MPa
170000 psi
Tensile Strength, Yield 1034 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
Elongation at Break 10 %
10 %
Reduction of Area 32 %
32 %
Component Elements Properties Metric English Comments
Carbon, C 0.18 %
0.18 %
Chromium, Cr 13 %
13 %
Iron, Fe 81 %
81 %
as balance
Manganese, Mn 0.25 %
0.25 %
Nickel, Ni 2.0 %
2.0 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.015 %
0.015 %
Tungsten, W 3.0 %
3.0 %