Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is best suited for narrow gap situations (.001"-.005" clearance). Handy Flux, Handy Flux Type B-1 or dispensable Handy Flux Types D or DB should be used with this filler metal. Applications:Braze 380 is a good general purpose low temperature brazing filler metal for use in cadmium-free brazing applications, such as air conditioning and refrigeration which involve the joining of steels, copper, copper alloys and nickel alloys.Specifications:Braze 380 is made to conform to the following specifications- AWS 5.8 BAg-34, Boiler & Pressure Vessel Code Sec II-C BAg-34, SAE AMS-4761 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.06 g/cc
0.327 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 214 - 228 MPa
31000 - 33000 psi
Copper butt joint
241 - 310 MPa
35000 - 45000 psi
Brass butt joint
379 - 448 MPa
55000 - 65000 psi
Low Carbon Steel butt joint
552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Elongation at Break 2.0 - 5.0 %
2.0 - 5.0 %
% in 2", 304 Stainless Steel butt joint
8.0 - 13 %
8.0 - 13 %
% in 2", Low Carbon Steel butt joint
15 - 30 %
15 - 30 %
% in 2", Brass butt joint
25 - 35 %
25 - 35 %
% in 2", Copper butt joint
Thermal Properties Metric English Comments
Melting Point 649 - 721 °C
1200 - 1330 °F
Solidus 649 °C
1200 °F
Melting Point
Liquidus 721 °C
1330 °F
Flow Point
Component Elements Properties Metric English Comments
Copper, Cu 31 - 33 %
31 - 33 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 37 - 39 %
37 - 39 %
Tin, Sn 1.5 - 2.5 %
1.5 - 2.5 %
Zinc, Zn 26 - 30 %
26 - 30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000950 ohm-cm
0.00000950 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 721 - 816 °C
1330 - 1500 °F
Brazing Range
Descriptive Properties Value Comments
Color Pale Yellow