Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.550 J/g-°C @Temperature 500 °C |
0.131 BTU/lb-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Specific Heat Capacity | 0.548 J/g-°C @Temperature 500 °C |
0.131 BTU/lb-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Specific Heat Capacity | 0.550 J/g-°C @Temperature 500 °C |
0.131 BTU/lb-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Specific Heat Capacity | 0.550 J/g-°C @Temperature 500 °C |
0.131 BTU/lb-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
Specific Heat Capacity | 0.549 J/g-°C @Temperature 652 °C |
0.131 BTU/lb-°F @Temperature 1210 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
Specific Heat Capacity | 0.550 J/g-°C @Temperature 20.0 - 300 °C |
0.131 BTU/lb-°F @Temperature 68.0 - 572 °F |
|
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |
|||
Specific Heat Capacity | 0.550 J/g-°C @Temperature 500 °C |
0.131 BTU/lb-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |