Material Notes:
Scotchkote Epoxy Sceed RS 820 has been specially developed as a three component 100% solids resurfacing screed for application to concrete floor surfacesProduct Features:Combines good application characteristics with excellent chemical resistanceDesigned for application by trowel for floatCan be used to form wall/floor covings and can be laid to fails. Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness 6100 microns
240 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 75 - 80
75 - 80
ASTM D2240
Tensile Strength at Break 22.6 MPa
3280 psi
ASTM D638
Elongation at Break 15 - 20 %
15 - 20 %
ASTM D412
Compressive Strength 86.2 MPa
12500 psi
ASTM D695
Impact Test 1.40 J
1.03 ft-lb
ASTM D2794
Abrasion 78
78
[mg] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Light Gray