Material Notes:
3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT40 is a low viscosity high temperature resistant toughened cyanocylate that works well with close-fitting parts.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 40 cP
40 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 106 °C
223 °F
Continuous
121 °C
250 °F
Intermittent
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Continuous
-54.0 °C
-65.2 °F
Intermittent
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.333 min
0.00139 - 0.00555 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid