Teknor Apex APEX® 80328 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 80328 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 80°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 85
85
10 seconds; ASTM D2240
Tensile Strength at Break 16.2 MPa
2350 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use; ASTM D794
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Oxygen Index 23 %
23 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.62

@Frequency 1.00e+6 Hz
3.62

@Frequency 1.00e+6 Hz
ASTM D150
5.22

@Frequency 1000 Hz
5.22

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.067

@Frequency 1000 Hz
0.067

@Frequency 1000 Hz
ASTM D150
0.14

@Frequency 1.00e+6 Hz
0.14

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque