3M FP02680N White Polypropylene Label Products

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FP02680N White Polypropylene Label Products.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ White Polypropylene Label Products FP02680 is a white opaque material that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tackified acrylic formulate for acid resistance and adhesion to polyolefins.Information provided by 3M
Physical Properties Metric English Comments
Thickness 2.54 microns
0.100 mil
Liner
58.4 microns
2.30 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.877 kN/m
5.00 pli
180° Peel 12"/min, 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
60.0 °C
140 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
5.00 °C
41.0 °F
Application
Descriptive Properties Value Comments
Adhesive Type P1480 Perm 24
Liner Clear Polyester Liner