Polymer Property : Melt Index of Compound = 8.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 3.5 - 8.5 g/10 min

@Load 5.00 kg,
Temperature 265 °C
3.5 - 8.5 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
3M Dyneon™ THV 510ESD Fluorothermoplastic  (discontinued **)
THV 510ESD is a flexible, fluoroplastic compound composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature proces..