3M 3340 HVAC Construction

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3340 HVAC Construction.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aluminum foil tape, for use with rigid and flexible ducts. UL 181 A-P and 181 B-FX Listed.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3652
102 microns
4.00 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.3 MPa
4970 psi
ASTM D3759
Peel Strength 0.3287 kN/m
1.875 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic