Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Recommended |
Nye Lubricants 670 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
Chesterton 785 Parting Lubricant Description: Chesterton® 785 Parting Lubricant represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless sy.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
ChevronTexaco Delo® NLGI 00 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | See Note 1. |
ChevronTexaco Multifak® EP NLGI Grade 2 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | JIS-K-6723 |
Denka VINYKON W2035 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | JIS-K-6723 |
Denka VINYKON W2086 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3340 HVAC Construction Aluminum foil tape, for use with rigid and flexible ducts. UL 181 A-P and 181 B-FX Listed.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3350 HVAC Construction Polypropylene tape for use with flexible ducts. UL 181 B-FX ListedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3380 General Purpose Aluminum Foil Tape 40 lb natural kraft paper liner. Good for narrow slit rolls. UL 723 ClassifiedInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3380 HVAC Construction General purpose aluminum foil tape. Go to product for this market. UL 723 Classified.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 33806 Premium Performance Aluminum Foil Tape High temperature acrylic adhesive of 425°FInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 34383 General Purpose Aluminum Foil Tape General purpose aluminum foil tapeInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ5216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ5201 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ6344 Protective Product, Molded Shapes 3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 4201 Lead Foil Tape Permanent acrylic adhesiveInformation provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 5423 Polyethylene Tape 3M™ Polyethylene Tape 5422 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ5000 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 97065 General Purpose Aluminum Foil Tape 60 lb. moisture stable liner. Good for die-cut applications.Information provided by 3M |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
3M SJ5202 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
ChevronTexaco Rykon® NLGI 1 Premium Grease EP FeaturesChevron Rykon Premium Grease EP is a high quality, water resistant, extreme pressure, multipurpose lubricating grease.It is manufactured using highly refined, select high viscosity index bas.. |
|||
Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | |
3M 3383 Premium Performance Aluminum Foil Tape 66 lb. moisture stable liner.Information provided by 3M |