Dow Corning X3-6211 ENCAPSULANT

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning X3-6211 ENCAPSULANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, clear, UV cure.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc

@Temperature 25.0 °C
0.990 g/cc

@Temperature 77.0 °F
Viscosity 930 cP
930 cP
dynamic
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 45
45
Thermal Properties Metric English Comments
CTE, linear 430 µm/m-°C
239 µin/in-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -80.0 °C
-112 °F
Electrical Properties Metric English Comments
Dielectric Strength 16.5 kV/mm
420 kV/in
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance clear
Gel Hardness (Grams/Penetration) 120
Hydrophobic yes
Self Leveling yes
Water Resistant yes