Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.65 - 1.85 g/cc
0.0596 - 0.0668 lb/in³
Molded
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 20 - 30
20 - 30
Tensile Strength 49.6 - 63.4 MPa
7200 - 9200 psi
Flexural Strength 89.6 - 117 MPa
13000 - 17000 psi
Flexural Modulus 6.21 - 7.58 GPa
900 - 1100 ksi
Compressive Strength 71.0 - 98.6 MPa
10300 - 14300 psi
Izod Impact, Notched 2.83 - 3.90 J/cm
5.30 - 7.30 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C
425 - 500 °F
Flammability, UL94 HB
HB
This product is not currently UL listed.
Electrical Properties Metric English Comments
Dielectric Strength 16.5 - 18.4 kV/mm
418 - 468 kV/in
short time
Arc Resistance 143 sec
143 sec
Processing Properties Metric English Comments
Processing Temperature 143 - 171 °C
290 - 340 °F