Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 5.00e+7 ohm @Diameter 8.00 - 10.0 mm |
5.00e+7 ohm @Diameter 0.315 - 0.394 in |
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environmen.. |
|||
Insulation Resistance | >= 5.00e+7 ohm | >= 5.00e+7 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe PF CC 204 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts.Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+7 ohm | >= 5.00e+7 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe PF CP 203 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+7 ohm @Diameter 8.00 - 10.0 mm |
>= 5.00e+7 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+7 ohm | >= 5.00e+7 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe PF CC 202 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm).Information provided by Hippe. |
|||
Insulation Resistance | 5.00e+7 - 5.00e+11 ohm | 5.00e+7 - 5.00e+11 ohm | Average value: 1.47e+11 ohm Grade Count:20 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |