Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes

Category Polymer , Thermoset , Phenolic
Manufacturer Elektro-Isola
Trade Name Etronax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environments. Can be lubricated with water, oil or grease.Applications: Ball-bearing cages for spindle bearings and guide rings for hydraulic cylinders. Can be used in particular, for mechanical applications where fine tolerances and smooth surface finish are required.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.30 g/cc

@Thickness >=0.000 mm
0.0470 lb/in³

@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Water Absorption 0.25 %
0.25 %
24hr/50°C+24hr in water at 23°C; ISO 62-1; IEC/EN 61212-2 7.2
Mechanical Properties Metric English Comments
Flexural Strength 120 MPa

@Diameter >=100 mm
17400 psi

@Diameter >=3.94 in
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1
Compressive Strength 170 MPa

@Temperature 23.0 °C,
Time 86400 sec
24700 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Adhesive Bond Strength 150 MPa

@Diameter <=100 mm
21800 psi

@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 100 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
212 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 5.00e+7 ohm

@Diameter 8.00 - 10.0 mm
5.00e+7 ohm

@Diameter 0.315 - 0.394 in
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2
Dielectric Strength 0.400 kV/mm

@Thickness 3.00 mm
10.2 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
0.800 kV/mm

@Diameter >=3.00 mm
20.3 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Users viewing this material also viewed the following: