Material Notes:
Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm).Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.40 g/cc
1.30 - 1.40 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 60.0 MPa
>= 8700 psi
IEC 1212-2 5.7
Flexural Strength >= 90.0 MPa
>= 13100 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 7.00 GPa
>= 1020 ksi
IEC 1212-2 5.2
Shear Strength >= 20.0 MPa
>= 2900 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 5.90 kJ/m²
>= 2.81 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 0.780 J/cm²
>= 3.71 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+7 ohm
>= 5.00e+7 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.5

@Frequency 48.0 - 62.0 Hz
<= 5.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 20000 V

@Temperature 90.0 °C
>= 20000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Comparative Tracking Index >= 100 V
>= 100 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 120 T.I.
IEC 1212-2 7.1
Water Absorption < 209 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm