Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod

Category Polymer , Thermoset , Epoxy , Epoxy, Molded, Glass Fiber Filler
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.40 g/cc
1.20 - 1.40 g/cc
IEC 1212-2 7.2
Mechanical Properties Metric English Comments
Flexural Strength >= 125 MPa

@Diameter >=100 mm
>= 18100 psi

@Diameter >=3.94 in
Perpendicular to laminations; IEC 1212-2 4.1
Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+7 ohm

@Diameter 8.00 - 10.0 mm
>= 5.00e+7 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Dielectric Breakdown >= 30000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.00556 hour
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
>= 30000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 30000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Descriptive Properties Value Comments
Thermal Endurance 130 T.I.
IEC 1212-2 7.1
Water Absorption < 2 mg/cm²
IEC 1212-2 7.1