Polymer Property : Insulation Resistance = 5.00e+11 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 5.00e+7 - 5.00e+11 ohm
5.00e+7 - 5.00e+11 ohm
Average value: 1.47e+11 ohm Grade Count:20
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..