Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 533 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
ASTM D149
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
Conditioned; ASTM D149
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Dielectric Strength 21.0 kV/mm

@Thickness 3.18 mm
533 kV/in

@Thickness 0.125 in
Conditioned; ASTM D149
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
Dielectric Strength 21.0 kV/mm

@Thickness 3.18 mm
533 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Dielectric Strength 21.0 kV/mm

@Thickness 1.00 mm
533 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East)
VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts.
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East)
15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East)
15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East)
XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility.
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.1%); ASTM-D149
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.25%); ASTM-D149
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.0%); ASTM-D149
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.4%); ASTM-D149
Toyobo GLAMIDE® TY-791HT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
continuous tension; ASTM D149-75
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
Dielectric Strength 21.0 kV/mm

@Thickness 1.60 mm
533 kV/in

@Thickness 0.0630 in
continuous tension; ASTM D149-75
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group
Dielectric Strength 21.0 kV/mm

@Thickness 2.00 mm
533 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..