Parker Chomerics CHO-SEAL 1224 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL 1224 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.05 - 3.95 g/cc
3.05 - 3.95 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 72
58 - 72
ASTM D2240
Tensile Strength at Break >= 2.07 MPa
>= 300 psi
ASTM D412
Elongation at Break 200 - 500 %
200 - 500 %
ASTM D412
Tear Strength 8.75 kN/m
49.9 pli
ASTM D624
Compression Set 45 %

@Temperature 100 °C,
Time 252000 sec
45 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
Thermal Properties Metric English Comments
Thermal Conductivity 2.80 W/m-K

@Pressure 2.07 MPa
19.4 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Flex TR10; ASTM D1329
Electrical Properties Metric English Comments
Volume Resistivity 0.0020 ohm-cm
0.0020 ohm-cm
as supplied without pressure sensitive adhesive; MIL-DTL-83528
0.010 ohm-cm
0.010 ohm-cm
Post Tensile Set; MIL-DTL-83528 Para.4.6.9
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
>= 120 dB

@Frequency 1.00e+8 Hz
>= 120 dB

@Frequency 1.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 120 dB

@Frequency 5.00e+8 Hz
>= 120 dB

@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 120 dB

@Frequency 2.00e+9 Hz
>= 120 dB

@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 120 dB

@Frequency 1.00e+7 Hz
>= 120 dB

@Frequency 1.00e+7 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
Descriptive Properties Value Comments
Binder Silicone
EMP Survivability >0.9 kA / in
MIL-DTL-83528 Para.4.6.16
Filler Ag
Heat Aging <0.01ohm-cm
MIL-DTL-83528 Para.4.6.15
Type E
MIL-DTL-83528
Vibration Resistance, After <0.002 ohm-cm
MIL-DTL-83528 Para.4.6.13
Vibration Resistance, During <0.01 ohm-cm
MIL-DTL-83528 Para.4.6.13