Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 70 - 80 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
70 - 80 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 60 - 80 dB @Frequency 4.00e+9 - 1.80e+10 Hz |
60 - 80 dB @Frequency 4.00e+9 - 1.80e+10 Hz |
|
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding Description: Master Bond MB600S is a silver containing aqueous based sodium silicate system used as a coating in situations where EMI shielding effectiveness is paramount. Electromagnetic interferen.. |