Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics Tecknit
Trade Name Consil®-V
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.479 - 1.921 g/cc
1.479 - 1.921 g/cc
ASTM D792
Deformation 10 %
10 %
0.25 pli
20 %
20 %
0.45 pli
30 %
30 %
1.3 pli
40 %
40 %
3.3 pli
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 60
40 - 60
ASTM D2240
Tensile Strength >= 0.689 MPa
>= 100 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.050 ohm-cm
<= 0.050 ohm-cm
Shielding Effectiveness 70 dB

@Frequency 1.00e+9 Hz
70 dB

@Frequency 1.00e+9 Hz
Plane Wave
75 dB

@Frequency 1.00e+7 Hz
75 dB

@Frequency 1.00e+7 Hz
E-Field
80 dB

@Frequency 100000 Hz
80 dB

@Frequency 100000 Hz
H-Field
Descriptive Properties Value Comments
Binder Modified Silicone
Color Tan
Filler Silver-plated glass