Material Notes:
Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.634 g/cc
0.05903 lb/in³
Water Absorption 1.1 %
1.1 %
Mechanical Properties Metric English Comments
Flexural Strength 55.0 MPa
7980 psi
Compressive Strength 103 MPa
14900 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+8 ohm-cm
3.00e+8 ohm-cm
Dielectric Strength 20.0 kV/mm
508 kV/in
Arc Resistance 135 sec
135 sec