Surface Resistivity per Square 800 - 1000 ohm
800 - 1000 ohm
prints from standard 140/31 screen
Heraeus Cleviosâ„¢ S HT Antistatic/Conductive Polymer Coating for Screen Printing
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Cleviosâ„¢ S HT grade ..