Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10 - 18 ohm | 10 - 18 ohm | Coating |
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst.. |
|||
Surface Resistivity per Square | 10 - 18 ohm | 10 - 18 ohm | |
Parker Chomerics Tecknit Teckfilm™ Transparent Conductive Coating on Polyester Film Description: TECKFILM is a highly conductive coating deposited on a transparent polyester film. It is available in rolls 30" wide. Usable width is 28". The conductive coating is overcoated with a ce.. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PF-30CF/15T Polysulfone, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Techmer ES Electrafil® J-1/CF/40 BK PA66 |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Techmer ES Electrafil® J-1/CF/40 NAT PA66 |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Techmer ES Electrafil® J-1200/CF/20 NAT ABS |
|||
Surface Resistivity per Square | 10 - 12 ohm | 10 - 12 ohm | Sheet |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |