Material Notes:
AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive substrates. AA-DUCT AD1 shows slight settling when stored for a long period of time, no caking and will re disperse to a smooth homogeneous state. AA-DUCT AD1 formulation produces electrically conductive paths on a wide variety of surfaces including plastics, rubber, cloth, thermoplastic, paper, wood and many others. AA-DUCT AD1 designed for use in diversified applications as microwave EMI & RFI shielding, in the assembly or repair of printed circuit boards, wave-guides, electronic modules, flat cable, static shielding, connections, and circuitry.Appearance: SilverCure Type: Heat cure Benefits:High strengthPerfect bondEMI & RFI shieldingWave guides Substrates: Excellent choice for Integrated Circuits, aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards. Typical Application: Microwave EMI & RFI shielding, in the assembly or repair of printed circuit boards, wave-guides, electronic modules, flat cable, static shielding, connections, and circuitry.Catalyst: AnhydrideInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.35 g/cc
2.35 g/cc
Viscosity 6800 cP
6800 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Modulus of Elasticity 4.14 GPa
600 ksi
Poissons Ratio 0.35
0.35
Shear Strength 13.8 MPa
2000 psi
Lap
Adhesive Bond Strength 10.3 MPa
1500 psi
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 41.8 W/m-K
290 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
338 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Component Elements Properties Metric English Comments
Silver, Ag 70 - 72 %
70 - 72 %
Electrical Properties Metric English Comments
Surface Resistivity per Square 10 - 12 ohm
10 - 12 ohm
Sheet
Processing Properties Metric English Comments
Cure Time 42.0 min

@Temperature 200 °C
0.700 hour

@Temperature 392 °F
90.0 min

@Temperature 180 °C
1.50 hour

@Temperature 356 °F
150 min

@Temperature 160 °C
2.50 hour

@Temperature 320 °F
Pot Life 259200 min
259200 min
uncured
388800 min
388800 min
uncured, refrigerated
Shelf Life 6.00 Month
6.00 Month
uncured