Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.10 - 100 ohm | 0.10 - 100 ohm | |
Nanosonic Metal Rubber™ Metal Rubber™ is a unique self-assembled nanocomposite material that combines the high electrical conductivity of metals with the low mechanical modulus of elastomers. Self-assembly processing allo.. |
|||
Surface Resistivity per Square | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistivity per Square | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistivity per Square | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
PolyOne Stat-Tech™ PI-30GF/15SS Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Electrically ConductiveGlass Fiber ReinforcedStainless Steel Fiber FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Lubri-Tech™ PF-30CF/15T Polysulfone, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Techmer ES Electrafil® J-1/CF/40 BK PA66 |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Techmer ES Electrafil® J-1/CF/40 NAT PA66 |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Techmer ES Electrafil® J-1200/CF/20 NAT ABS |
|||
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D257 |
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |