Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 7.85e+15 ohm | 7.85e+15 ohm | |
Abatron AboCast 50-11/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours.. |
|||
Surface Resistance | 7.85e+15 ohm | 7.85e+15 ohm | |
Abatron AboCast 50-3/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | |
Abatron AboCast 50-6/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months. |
|||
Surface Resistance | 7.85e+15 ohm | 7.85e+15 ohm | |
Abatron AboCast 8103-11 One Part Epoxy One component system. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At.. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | Cond. A |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | C 96/23/96 |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | Cond. A |
Abatron AboCast 8504-1 One-Component Epoxy AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | C 96/23/96 |
Abatron AboCast 8504-1 One-Component Epoxy AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications. |
|||
Surface Resistance | 7.85e+15 ohm | 7.85e+15 ohm | |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |
|||
Surface Resistance | 7.85e+15 ohm | 7.85e+15 ohm | |
Abatron AboCast 50-16/AboCure 50-12 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours.. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | |
Abatron AboCast 50-16/AboCure 50-17 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at .. |
|||
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | |
Abatron AboCast 50-3/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months. |