Material Notes:
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).
Physical Properties Metric English Comments
Viscosity Measurement 100
100
Mechanical Properties Metric English Comments
Hardness, Rockwell M 87
87
Tensile Strength, Ultimate 65.29 MPa
9470 psi
Elongation at Break 8.1 %
8.1 %
Flexural Yield Strength 93.91 MPa
13620 psi
Flexural Modulus 2.84 GPa
412 ksi
Compressive Yield Strength 87.49 MPa
12690 psi
Compressive Modulus 1.97 GPa
286 ksi
Izod Impact, Notched 0.219 J/cm
0.410 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 64.0 °C
147 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.19e+16 ohm-cm
>= 1.19e+16 ohm-cm
Surface Resistance 7.85e+15 ohm
7.85e+15 ohm
Dielectric Constant 3.24

@Frequency 1e+6 Hz
3.24

@Frequency 1e+6 Hz
3.62

@Frequency 1000 Hz
3.62

@Frequency 1000 Hz
3.67

@Frequency 60 Hz
3.67

@Frequency 60 Hz
Dissipation Factor 0.0098

@Frequency 60 Hz
0.0098

@Frequency 60 Hz
0.013

@Frequency 1000 Hz
0.013

@Frequency 1000 Hz
0.025

@Frequency 1e+6 Hz
0.025

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 38 min
38 min
500 g
Descriptive Properties Value Comments
Exotherm 280°C
Peak
Copyright © lookpolymers.com All Rights Reserved