Material Notes:
AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications.
Physical Properties Metric English Comments
Viscosity 12000 cP
12000 cP
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
Tensile Strength at Break 29.0 MPa
4200 psi
Elongation at Break 1.1 %
1.1 %
Flexural Strength 82.7 MPa
12000 psi
Flexural Modulus 2.76 GPa
400 ksi
Compressive Strength 215 MPa
31200 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 168 °C
334 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 9.63e+15 ohm-cm
9.63e+15 ohm-cm
"A"
1.22e+16 ohm-cm
1.22e+16 ohm-cm
C 96/23/96
Surface Resistance >= 7.85e+15 ohm
>= 7.85e+15 ohm
Cond. A
>= 7.85e+15 ohm
>= 7.85e+15 ohm
C 96/23/96
Dielectric Constant 3.15

@Frequency 1.00e+6 Hz
3.15

@Frequency 1.00e+6 Hz
A
3.36

@Frequency 60.0 Hz
3.36

@Frequency 60.0 Hz
A
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 150 - 160 °C
1.00 - 2.00 hour

@Temperature 302 - 320 °F
60.0 - 240 min

@Temperature 160 - 180 °C
1.00 - 4.00 hour

@Temperature 320 - 356 °F
optional
Pot Life 200 min

@Temperature 100 °C
200 min

@Temperature 212 °F
Shelf Life 5.00 - 8.00 Month
5.00 - 8.00 Month