Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 1.00e+8 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+8 - 2.00e+17 ohm-cm
1.00e+8 - 2.00e+17 ohm-cm
Average value: 1.62e+16 ohm-cm Grade Count:173
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Electrical Resistivity 1.00e+8 - 1.00e+15 ohm-cm

@Temperature 66.0 - 130 °C
1.00e+8 - 1.00e+15 ohm-cm

@Temperature 151 - 266 °F
Average value: 7.80e+13 ohm-cm Grade Count:7
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
Electrical Resistivity 1.00e+8 - 5.80e+15 ohm-cm

@Temperature 30.0 - 400 °C
1.00e+8 - 5.80e+15 ohm-cm

@Temperature 86.0 - 752 °F
Average value: 1.21e+15 ohm-cm Grade Count:7
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Electrical Resistivity 1.00e+8 - 1.00e+15 ohm-cm
1.00e+8 - 1.00e+15 ohm-cm
Average value: 7.50e+14 ohm-cm Grade Count:11
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Electrical Resistivity 1.00e+8 - 1.00e+15 ohm-cm
1.00e+8 - 1.00e+15 ohm-cm
Average value: 8.57e+14 ohm-cm Grade Count:7
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Electrical Resistivity <= 1.00e+8 ohm-cm
<= 1.00e+8 ohm-cm
Magyar Aluminum ALOLT 60F Aluminum Hydroxide
Fine Precipitated Type
Electrical Resistivity 1.00e+8 - 1.00e+12 ohm-cm
1.00e+8 - 1.00e+12 ohm-cm
undoped
Mateck Zinc Sulphide, ZnS
Semiconductor single crystals. Twins and stacking faults < 4% of hexagonal phase.
Electrical Resistivity 1.00e+8 - 1.00e+12 ohm-cm
1.00e+8 - 1.00e+12 ohm-cm
BACT Dylyn® Diamond-Like Nanocomposite Coating
a-C:H/a-Si:O nanocomposite. This coating provides the lowest friction of the BACT products, even in high humidity or wet environments. It offers an excellent combination of anti-stick and wear be..
Electrical Resistivity 1.00e+8 ohm-cm

@Temperature 600 °C
1.00e+8 ohm-cm

@Temperature 1110 °F
Anderman Ceramics EA998 Sintered Alumina, 99.8%
High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1..
Electrical Resistivity 1.00e+8 - 1.00e+15 ohm-cm
1.00e+8 - 1.00e+15 ohm-cm
Average value: 3.02e+14 ohm-cm Grade Count:14
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Electrical Resistivity 1.00e+8 - 1.00e+17 ohm-cm
1.00e+8 - 1.00e+17 ohm-cm
Average value: 1.90e+15 ohm-cm Grade Count:64
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Electrical Resistivity 1.00e+8 - 9.90e+10 ohm-cm
1.00e+8 - 9.90e+10 ohm-cm
Average value: 2.02e+10 ohm-cm Grade Count:6
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Electrical Resistivity 1.00e+8 - 1.00e+12 ohm-cm
1.00e+8 - 1.00e+12 ohm-cm
undoped
Mateck Zinc Selenide, ZnSe
Semiconductor single crystals. Twins and stacking faults twin free.