Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+8 - 5.80e+15 ohm-cm @Temperature 30.0 - 400 °C |
1.00e+8 - 5.80e+15 ohm-cm @Temperature 86.0 - 752 °F |
Average value: 1.21e+15 ohm-cm Grade Count:7 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |