Material Notes:
Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.
Physical Properties Metric English Comments
Density 7.90 g/cc
0.285 lb/in³
RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 570 MPa
82700 psi
Outokumpu Typical, Cold Rolled Narrow Strip; EN 10002-1
Tensile Strength, Yield 220 MPa

@Strain 0.200 %
31900 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
250 MPa

@Strain 0.200 %
36300 psi

@Strain 0.200 %
Outokumpu Typical,Cold Rolled Narrow Strip; EN 10002-1
280 MPa

@Strain 1.00 %
40600 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Narrow Strip; EN 10002-1
98.0 MPa

@Strain 0.200 %,
Temperature 400 °C
14200 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
127 MPa

@Strain 0.200 %,
Temperature 200 °C
18400 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
155 MPa

@Strain 0.200 %,
Temperature 100 °C
22500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 50 %
50 %
Outokumpu Typical, Cold Rolled Narrow Strip; EN 10002-1
Modulus of Elasticity 200 GPa
29000 ksi
RT
172 GPa

@Temperature 400 °C
24900 ksi

@Temperature 752 °F
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 100 °C
8.89 µin/in-°F

@Temperature 212 °F
17.5 µm/m-°C

@Temperature 400 °C
9.72 µin/in-°F

@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C
0.120 BTU/lb-°F
RT
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
RT
20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 17.7 %
17.7 %
Iron, Fe 69.76 %
69.76 %
Nickel, Ni 12.5 %
12.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT
Users viewing this material also viewed the following: