Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Star Plastics PC721HFR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Star Plastics PC7523R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers |
|||
Melt Temperature | 95.0 - 302 °C | 203 - 575 °F | Average value: 186 °C Grade Count:31 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 274 - 302 °C | 525 - 575 °F | |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified