Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |