Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable 1800-xx19D Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable Y152 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 179 °C
340 - 354 °F
PolyOne Geon™ Vinyl Flexible R246AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 182 °C
340 - 360 °F
Huntsman PE1037 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con..
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 182 °C
340 - 360 °F
LyondellBasell Petrothene® YR19548 Polyolefin Compound
ApplicationsPETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance ..
Melt Temperature 171 - 182 °C
340 - 360 °F
Sylvin Technologies 8600-90 Clear PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 171 - 182 °C
340 - 360 °F
Sylvin Technologies 8960-90 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 171 - 182 °C
340 - 360 °F
Sylvin Technologies 9604-90 LMW Clear PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Melt Temperature 171 - 182 °C
340 - 360 °F
Sylvin Technologies 9940-90 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 171 - 182 °C
340 - 360 °F
Sylvin Technologies 9980-90 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 171 °C
340 °F
Teknor Apex APEX® 3201-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Melt Temperature 171 °C
340 °F
Teknor Apex APEX® 3211-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Melt Temperature 171 - 193 °C
340 - 380 °F
Processing Temperature
Teknor Apex Medalist® MD-120 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Melt Temperature 171 - 193 °C
340 - 380 °F
Processing Temperature
Teknor Apex Medalist® MD-160 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Melt Temperature 171 - 193 °C
340 - 380 °F
Processing Temperature
Teknor Apex Medalist® MD-235 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Melt Temperature 171 - 182 °C
340 - 360 °F
Molding
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l..
Melt Temperature 171 - 193 °C
340 - 380 °F
RTP Company RTP 2099 X 121249 A Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 88% Renewable Resource Content
Nucleated for high heat exposure.  For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website.
Melt Temperature 171 - 188 °C
340 - 370 °F
RTP Company RTP 2099 X 124789 C Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 84% Renewable Resource Content
Not optically transparent.  Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website.
Melt Temperature 171 - 193 °C
340 - 380 °F
RTP Company RTP 2099 X 124790 A Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast Cycle Nucleator - 78% Renewable Resource Content
Nucleated for high heat exposure.  For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website.
Melt Temperature 171 - 193 °C
340 - 380 °F
RTP Company RTP 2099 X 126216 A Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 88% Renewable Resource Content
Nucleated for high heat exposure.  For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website.
Melt Temperature 171 - 193 °C
340 - 380 °F
RTP Company RTP 2099 X 126218 A Bio-Based Polylactic Acid (PLA); Impact Modified - 94% Renewable Resource Content
For detailed processing information, see the PLA Molding Guide on the RTP Company website.
Melt Temperature 171 °C
340 °F
Axiall 53080A Moldings & Extrusions Flexible PVC
General purpose molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 171 °C
340 °F
Axiall 8702 Moldings & Extrusions Flexible PVC
General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 171 °C
340 °F
Axiall 12792 Wire & Cable Flexible PVC
General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 171 °C
340 °F
Axiall 12850 Wire & Cable Flexible PVC
Flame retardant, UV resistant clear compound. Formulated for microbial resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 171 °C
340 °F
Axiall 8780 Moldings & Extrusions Flexible PVC
Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 171 °C
340 °F
Axiall 10750 Wire & Cable Flexible PVC
General purpose 75C jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 171 °C
340 °F
Teknor Apex APEX® 3202-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl..
Melt Temperature 171 °C
340 °F
Axiall 8681 Moldings & Extrusions Flexible PVC
General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.