Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0850-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0860-xx02D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1604-xx27FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable JLK51A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1800L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2302 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable WELB406L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable WELB406LU Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJB593KBL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y152 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y283 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 350 °F | Extrusion |
PolyOne Geon® XV3811B Thermoplastic Elastomer - PVC/TPU
(discontinued **) Applications:Hose and TubingCustom ProfilesProcessing Method:Extrusion and MoldingExtrusion-ProfileInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible R1211P Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8600-80 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8925-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8940-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8960-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9077-80 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9077-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9600-80 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9950-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9980-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9812A-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |