PolyOne Geon™ Vinyl Flexible R351AE Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible R351AE Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
15 sec; ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 15.9 MPa

@Strain 100 %
2310 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 280 %
280 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 101 kN/m
576 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 171 - 179 °C
340 - 354 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Features General Purpose
Low Temperature Resistant
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Profile Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Flooring
Furniture
General Purpose
Profiles