Polymer Property : Melt Temperature = 351 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 168 - 177 °C
334 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable 0850-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 168 - 177 °C
334 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable 0860-xx02D Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable 1604-xx27FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable 1800-xx19D Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable JLK51A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable W1800L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable W2302 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable WELB406L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable WELB406LU Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable WJB593KBL Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable WJLK61 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable Y152 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Wire & Cable Y283 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible FC700 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible R109AM Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 166 - 177 °C
331 - 351 °F
PolyOne Geon™ Vinyl Flexible R7542X Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible C7000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 168 - 177 °C
334 - 351 °F
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible R1211P Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 171 - 177 °C
340 - 351 °F
PolyOne Geon™ Vinyl Flexible R355AM Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Melt Temperature 163 - 177 °C
325 - 351 °F
Huntsman PE1507 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..