ExxonMobil Paxon™ AB50-003 Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Paxon™ AB50-003 Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: No Applications: Food packagingHousehold and Industrial chemical containersPharmaceutical PackagingThermoformed Parts Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
ESCR 100% Igepal® 70 hour
70 hour
ASTM D1693 Condition B
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 189 kJ/m²
90.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F