Axiall 1063-119i Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 1063-119i Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Highly flame retardant CMR jacket for use over HDPE inners in 20-22 mil wall applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.53 - 1.57 g/cc
1.53 - 1.57 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 44 - 50
44 - 50
delayed; ASTM D-2240
Tensile Strength, Yield 17.48 MPa
2535 psi
ASTM D-638
Elongation at Yield 207.5 %
207.5 %
Air Aging: 7 days @ 100°C; UL 1581
250 %
250 %
ASTM D-638
100% Modulus 0.01547 GPa
2.244 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Oxygen Index 39 %
39 %
ASTM D-638
Electrical Properties Metric English Comments
Dielectric Constant 3.47

@Frequency 1e+6 Hz
3.47

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F