Material Notes:
Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excellent thermal stability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 52.9 MPa
7670 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.62 GPa
380 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 94.5 MPa
13700 psi
ASTM D790
Flexural Modulus 2.73 GPa
396 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.44 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 3.18 mm
212 °F

@Thickness 0.125 in
Unannealed; ASTM D648
104 °C

@Thickness 3.18 mm
219 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 191 - 202 °C
376 - 396 °F
Descriptive Properties Value Comments
Forms Pellets
Generic Material CPVC
Generic Name Polyvinyl Chloride, Chlorinated (CPVC)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Interior Parts
Profiles
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved