Rear Barrel Temperature 221 - 249 °C
430 - 480 °F
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 221 - 232 °C
430 - 450 °F
Polymer Resources NY6/12-GP1 General Purpose Nylon 612
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized
General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated
General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Rear Barrel Temperature 221 - 254 °C
430 - 490 °F
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy
PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Rear Barrel Temperature 221 - 254 °C
430 - 490 °F
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 221 - 254 °C
430 - 490 °F
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Rear Barrel Temperature 221 - 254 °C
430 - 490 °F
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow
PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Rear Barrel Temperature 221 - 271 °C
430 - 520 °F
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Rear Barrel Temperature 221 - 229 °C
430 - 445 °F
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 221 - 229 °C
430 - 445 °F
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 221 - 229 °C
430 - 445 °F
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 221 - 249 °C
430 - 480 °F
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-IM1 Nylon 6, Impact Modified
Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized
Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
Rear Barrel Temperature 221 - 246 °C
430 - 475 °F
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 221 - 254 °C
430 - 490 °F
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow
PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Rear Barrel Temperature 221 - 254 °C
430 - 490 °F
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Rear Barrel Temperature 221 - 232 °C
430 - 450 °F
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black
Rear Barrel Temperature 221 °C
430 °F
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa..
Rear Barrel Temperature 221 - 249 °C
430 - 480 °F
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Rear Barrel Temperature 221 - 249 °C
430 - 480 °F
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose
Data provided by Clariant Masterbatches
Rear Barrel Temperature 221 - 249 °C
430 - 480 °F
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Rear Barrel Temperature 221 - 271 °C
430 - 520 °F
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.