Processing Properties Metric English Comments
Rear Barrel Temperature 221 - 229 °C
430 - 445 °F
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 221 - 229 °C
430 - 445 °F
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 221 - 229 °C
430 - 445 °F
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).