Polymer Property : Mold Temperature = 166 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 166 - 193 °C
331 - 379 °F
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability..
Mold Temperature 166 - 193 °C
331 - 379 °F
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr..
Mold Temperature 166 - 193 °C
331 - 379 °F
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Mold Temperature 166 - 193 °C
331 - 379 °F
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
Mold Temperature 166 - 193 °C
331 - 379 °F
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable..
Mold Temperature 166 - 193 °C
331 - 379 °F
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..