Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 130 - 177 °C | 266 - 350 °F | Average value: 154 °C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Mold Temperature | 130 - 177 °C | 266 - 350 °F | Average value: 151 °C Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Mold Temperature | 130 - 177 °C | 266 - 350 °F | Average value: 149 °C Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Mold Temperature | 130 - 177 °C | 266 - 350 °F | Average value: 153 °C Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Mold Temperature | 130 - 177 °C | 266 - 350 °F | Average value: 154 °C Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Mold Temperature | 130 - 177 °C | 266 - 350 °F | Average value: 152 °C Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Mold Temperature | 130 - 180 °C | 266 - 356 °F | Average value: 155 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Mold Temperature | 130 - 155 °C | 266 - 311 °F | For optimal surface finish |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
Mold Temperature | 130 - 155 °C | 266 - 311 °F | for optimal gloss and heat resistance |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Mold Temperature | 130 - 155 °C | 266 - 311 °F | For optimal surface finish |
Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled Crystalline Polymer, Glass Filled |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton CE/60 PPS, 60% Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; .. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Mold Temperature | 130 - 150 °C | 266 - 302 °F | |
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G.. |
|||
Mold Temperature | 130 - 150 °C | 266 - 302 °F | |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Mold Temperature | 130 - 150 °C | 266 - 302 °F | |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Mold Temperature | 130 - 150 °C | 266 - 302 °F | |
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Mold Temperature | 130 - 150 °C | 266 - 302 °F | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Mold Temperature | 130 - 160 °C | 266 - 320 °F | |
E-Polymers SEPAZ® K365GM 60% Glass Fiber/Calcium Carbonate Reinforced General Purpose PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
DuPont Performance Polymers Rynite® FG530 NC011 PET
(Unverified Data**) Rynite® FG530 NC011is a 30% glass fiber reinforced modified polyethylene terephthalate resin. It has been developed for consideration into applications for the food industry.Information provided by.. |