Polymer Property : Nozzle Temperature = 535 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 246 - 279 °C
475 - 535 °F
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 260 - 279 °C
500 - 535 °F
Solvay Technyl® A216V15 15% Glass Filled Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Nozzle Temperature 271 - 279 °C
520 - 535 °F
Solvay Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Nozzle Temperature 271 - 279 °C
520 - 535 °F
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Nozzle Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
Nozzle Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Nozzle Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade
Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W..
Nozzle Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St..
Nozzle Temperature 271 - 279 °C
520 - 535 °F
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Nozzle Temperature 268 - 279 °C
515 - 535 °F
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Nozzle Temperature 252 - 279 °C
485 - 535 °F
Teknor Apex Chemlon® 340G Nylon 610, Glass Fiber Reinforced
Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Nozzle Temperature 252 - 279 °C
485 - 535 °F
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced
Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Nozzle Temperature 271 - 279 °C
520 - 535 °F
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Nozzle Temperature 271 - 279 °C
520 - 535 °F
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Nozzle Temperature 263 - 279 °C
505 - 535 °F
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced
Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo..