Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in EuropeInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ISO 2781
Maximum Moisture Content 0.050
0.050
Melt Flow 10 - 25 g/10 min

@Load 8.70 kg,
Temperature 205 °C
10 - 25 g/10 min

@Load 19.2 lb,
Temperature 401 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868
Hardness, Shore D 50
50
ISO 868
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ISO 37
Elongation at Break 560 %
560 %
ISO 37
Tensile Modulus 0.0580 GPa
8.41 ksi
ISO 527
50% Modulus 0.0100 GPa
1.45 ksi
ISO 37
100% Modulus 0.0125 GPa
1.81 ksi
ISO 37
300% Modulus 0.0250 GPa
3.63 ksi
ISO 37
Rebound 43 %
43 %
ISO 4662
Tear Strength 117 kN/m
668 pli
with incision; ISO 34B
151 kN/m
862 pli
without incision; ISO 34B
Abrasion 33
33
mm<sup>3</sup>; ISO 4649
Compression Set 19 %
19 %
70 hrs./22°C; ISO 815
31 %
31 %
24 hrs./70°C; ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
A50; ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Injection
Nozzle Temperature 200 - 210 °C
392 - 410 °F
Injection
Zone 1 195 - 205 °C
383 - 401 °F
Injection
Zone 2 200 - 210 °C
392 - 410 °F
Injection
Zone 3 205 - 215 °C
401 - 419 °F
Injection
Zone 4 205 - 215 °C
401 - 419 °F
Injection
Drying Temperature 100 °C
212 °F
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Dew Point <= -30.0 °C
<= -22.0 °F
Users viewing this material also viewed the following: