Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase |
|||
Front Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Front Barrel Temperature | >= 227 °C | >= 440 °F | |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
PTS Trilac® ABS-HS7500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® D 4400 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 4001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, GoodCompressive Strength, GoodHeat Resistance, MediumOzone ResistantThermal Stability, GoodForms:PelletsProcessing Methods:Injection MoldingExtrusion Information pro.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 4001 LCS Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 7011 TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 7101 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 8030 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 8502 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Moldability, GoodPaintable Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsInforma.. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 9002 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Front Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Front Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc.. |
|||
Front Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Front Barrel Temperature | 227 - 274 °C | 440 - 525 °F | |
LTL Color Compounds ColorFast® JCT1000 Polycarbonate-ABS-SMA Alloy Unique PC/ABS/SMA alloy with improved processing and reduced plate-outAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 227 °C | 440 °F | |
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |